Skip to product information
1 of 5

Lab X Creations

FIBERLAM Plus 55 Gallon Polyester Resin; Low Viscosity Coating for Laminating Fiberglass mat/Biaxal/Cloth; Boat/RV/Automotive/Canoe/Surfboard| 24-36hr TACK Time

FIBERLAM Plus 55 Gallon Polyester Resin; Low Viscosity Coating for Laminating Fiberglass mat/Biaxal/Cloth; Boat/RV/Automotive/Canoe/Surfboard| 24-36hr TACK Time

Regular price $1,324.99 USD
Regular price $1,535.00 USD Sale price $1,324.99 USD
Sale Sold out
FLP55G-drum
  • 📦 Shipping: Contact us directly for shipping inquiries if your shipping address isn't already in our predefined freight rates system.
  • FORKLIFT: If you do not have a forklift or similar means to offload, there is a 50 dollar fee for liftgate service and residential also has a service charge as well.
  • ✅ GRADE A - Not a boatyard resin, our resin is much higher quality. This Polyester Fiberglass Laminating Resin is the highest grade you will find. A premium product used in the marine industry and by most RV and Boat manufacturers. Marine Grade Resin. 
  • CURES FULLY in 24-36hrs without wax - Use this resin on Wood, Fiberglass, or Metal without any hassle. Depending on temperature and humidity, it can reach its cured stage in as quick as 4 hours but may take up to 24-36 hours depending on amount of MEKP added or if temperatures are lower than 72°F, If temperatures are too low it will take even longer, humidity is also a factor.
  • CURES TACK FREE (no wax is present in this resin) after 24-36hrs - Manufactured in the USA, this Ortho-type resin cures tack free in 24-36hrs. For faster time to full cure / no tack; wax may be added to reduce tack time to less than 24hrs.
  • MULTIPLE APPLICATIONS - This polyester fiberglass resin is great for the following applications: marine, general purpose fiberglass laminating, aero space, FRP (Fiber Reinforced Plastic) parts, auto body, transportation, wood, and much more
  • HIGH COMPATIBILITY - Compatible with all types of Fiberglass and coring materials, including expanded PVC coring and so much more, this polyester laminating resin is perfect for high quality repairs, new construction parts, and vertical surface laminations.
  • From Water crafts to Bathrooms - Upgrade your building and repairs with our general-purpose marine fiberglass resin. You can confidently use it on a boat, surfboard, automobile, and even a bathtub or shower. Gelcoat adheres with a superior bond to this resin as well.
  • Mix Ratio chart is on the label for easy reference to mix according to your desired work time. MIX FULLY to ensure a complete and proper reaction. Scrape the sides of the container you are mixing in as well as the bottom to ensure a complete mix. Easy to spread, this high wetting resin impregnates fibrous material quickly and can be applied using spray guns or hand layups.
  • Excellent Tackiness - Our FiberLam Plus fiberglass resin stays tacky for a longer period. Allowing for easier application to stack layers of reinforcement materials (fiberglass), which creates a stronger adhesion, we recommend 3-5 laminations to be done per layup.
  • 🏢 Business pricing available, contact us of for details

 

Important Mixing & Application Guidelines:

  • Mix Thoroughly: Always scrape the sides and bottom of your container to ensure the resin and catalyst are 100% combined. Unmixed portions will leave uncured spots on your project. Use a smooth-sided container and avoid using drill mixing bits.
  • Work in Small Batches: Mix only what you can easily apply within 7 minutes. Start with a 1-pint batch to gauge your working time. Do not mix more than 1 to 2 quarts at once, as larger batches generate excess heat and cure prematurely.
  • Rough it up: sand or grind the surface to create clean and rough surface with a "tooth" for the resin to grab onto (a mechanical bond).
  • Clean it off: Before applying the resin, the surface must be completely wiped down with a solvent like acetone to remove dust, wax, and grease. The surface must be 100% dry before the resin touches it.
  • Summer Weather Adjustments: During hot summer months, consider reducing your catalyst ratio to 0.75% to extend your working time before the resin gels.
  • The Danger of "Hot Batches" (Over-Catalyzing): Adding too much catalyst causes an aggressive exothermic reaction. The resin can smoke, crack, warp the project, or even catch fire in the mixing cup.
  • Manage Sunlight: Avoid applying the resin in direct sunlight, which drastically accelerates the cure time. If it is over 75°F, work in the shade. Once the application is complete, you can move your project into the sun to help speed up the final curing process.
  • Moisture: Applying resin to damp wood or working in extremely high humidity/rainy conditions can inhibit the cure, causing the resin to stay cloudy or tacky. Everything must be bone dry.
  • Clean-Up Requires Acetone: be sure to routinely clean your tools, brushes and so on with acetone as it will dissolve the resin. Mineral Spirits and other cleaners are not effective.
  • Proper storage to maximize shelf life: store the resin and the MEKP catalyst in a cool, dark, and dry climate-controlled environment. Leaving it in a hot garage or freezing shed will ruin the product.
  • Coverage Estimate: As a general rule, 1 gallon of resin will wet out approximately 40–50 square feet of 1.5 oz chopped strand mat, or roughly 4 square yards of standard fiberglass cloth, depending on application thickness and technique.
  • Proper Safety Gear (PPE) is Non-Negotiable: 
    • Ventilation & Respirators: always work in a well-ventilated area and it is strongly recommend a respirator fitted with organic vapor cartridges be used.
    • Gloves: Gloves must be used, heavy duty gloves are encouraged. Nitrile gloves are okay, but latex tends to be better. The chemicals in polyester resin can break down cheaper nitrile, leaving hands exposed and sticky.
    • If exposed skin comes in contact with resin, catalyst or both. clean affected area immediately. Be very cautious in use of acetone anywhere on or near your body. Use soap and water and clean vigorously and thoroughly.